可以对你想要的颜色进行上色,但我们在对铝塑板上色时,难免会遇到染不上色的状况,那么,铝塑板染不上色的发生原
You can colour the color you want, but when we colour the aluminium plastic sheet, we will inevitably encounter the situation that the color cannot be dyed. Then, the origin of the color cannot be dyed on the aluminium plastic sheet.
因及处理方法有:
The causes and treatment methods are as follows:
1、阳极氧化膜厚不足:解决的办法是检查阳极氧化工艺是否规范,看温度,电压,导电等要素是否稳定,若有异
1. Insufficient thickness of anodic oxide film: The solution is to check whether the anodic oxidation process is standardized and whether the factors such as temperature, voltage and conductivity are stable, if different.
常,请相应调整规范之,若无异常,可恰当延长氧化时间,确保膜厚合格。
Often, please adjust the specifications accordingly. If there is no abnormality, the oxidation time can be prolonged appropriately to ensure that the film thickness is up to standard.
2、染液PH值太高:此刻,可用冰醋酸将PH值调至规范值。
2. The PH value of dye solution is too high: at this moment, the PH value can be adjusted to the standard value by glacial acetic acid.
3、氧化后工件在水槽中放置时间太久:发起及时染色,假如这种状况现已发生,可将工件放在阳极氧化槽中或硝
3. After oxidation, the workpiece is placed in the tank for too long: initiating timely dyeing, if this situation has occurred, the workpiece can be placed in the anodic oxidation tank or nitrate
酸中和槽中恰当活化处理后再进行染色,效果会很好。
Appropriate activation treatment in acid neutralization tank before dyeing can achieve good results.
4、选用染料已分解或霉变:此刻需更换染料,选用适宜染料。
4. Choose dyestuffs that have been decomposed or moulded. At this moment, dyestuffs need to be replaced and suitable dyestuffs should be selected.


5、氧化温度过低,导致皮膜致密:可恰当进步氧化温度。
5. Low oxidation temperature results in dense skin film: oxidation temperature can be properly improved.
6、导电不良:可能阳极铜杆或阴极铅板接触不良所示批量导电不良。留意清洗阳极铜杆及阴极铅板,确保导电良
6. Poor conductivity: Batch conductivity shown by poor contact of anode copper rod or cathode lead plate may be poor. Pay attention to cleaning anode copper rod and cathode lead plate to ensure good conductivity
好。
OK.
以上就是关于铝塑板染不上色的发生原因及处理方法,现在,铝塑板现已成为建筑范畴的常用材料,其广泛用于大楼
Above is about the causes and treatment methods of stainless aluminium-plastic sheet. Now, aluminium-plastic sheet has become a common building material, which is widely used in buildings.
外墙、室内墙面、广告招牌等装修用范畴。然而跟着人们对装修用品的美观要求越来越高,色彩单一、图画呆板的铝塑板
Exterior walls, interior walls, advertising signs and other decoration areas. However, along with people's increasingly high aesthetic requirements for decoration supplies, single color, stiff drawing of aluminum-plastic sheet
现已无法满意出产需求。